Partial dismantling as a method of removing laminate damages
Laminate is a very high quality and durable floor covering. But even such a durable and wear-resistant material is not insured for one hundred percent from the appearance of cracks, chips and cracks. There are such damages most often in the process of moving heavy furniture or from blows with something weighty, such as a fallen statuette.
There is a popular belief that the laminate can be repaired only by dismantling it to the point of damage. And this opinion has a right to exist, since, indeed, well-pronounced defects, it is possible to remove, only by such a radical method.
But before taking such a step, you should weigh the pros and cons, since there is a threat of damage to the coating even more, with inept dismantling. And then you have to replace the laminate throughout the room.
You can also use a less risky method. A damaged piece is cut out, and a new one is glued in its place.
How to fix a deep scratch in a laminate
If a deep scratch or chip is formed during the operation of this flooring, then do not worry, and you need to go shopping in the building store. There it is necessary to purchase a special repair composition for the laminate. Or, in case there was not one, the acrylic sealant, which needs to be chosen in two colors, is also suitable for later mixing them, giving the necessary shade. The choice of color should be carried out taking into account that when dried, the sealant will acquire a darker shade.
Once the purchases are made, it is possible to repair scratches and chips. To do this, prepare the mixture according to the instructions and use a rubber spatula to fill the groove in the floor.
This type of repair is recommended to use pointwise. If there are many scratches, it is better to replace the whole coating, because during repair it can lose its beautiful appearance, becoming untidy.
How to repair deep cracks and cracks in
laminate Such damages are sealed with a self-made solution of sawdust and gypsum mixed in a 1: 1 ratio, adding a little water to obtain a not too thick composition.
Next, you need to estimate the size of the gap, if it exceeds 6 cm, then one mixture will not be enough. To seal such large slots, you need a wooden bar to fit the crack, and you need to place it in it, and then fill the remaining space with the prepared mixture.
Elimination of blistering of individual fragments of laminate
Such swelling occurs when the surface is wet. Eliminates this problem by replacing the damaged slats.
You can buy new slats, or you can repair old ones. For this, swollen slats, put on a flat surface and press down with a heavy load and leave in this form for 5-7 days. When the strips take the right shape, they can be put back.
Restoring the old laminate floor
Since the laminate is very durable material, it can serve for many years. But over time, and especially after the repair, it can become dull and untidy. To fix this, you can cover it with floor lacquer, it will refresh its look and hide the repair area.